Open Access
| Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 19003 | |
| Number of page(s) | 6 | |
| Section | Posters: Mechanical Behavior I: Fatigue | |
| DOI | https://doi.org/10.1051/matecconf/20141419003 | |
| Published online | 8 octobre 2014 | |
- R. C. Reed, The Superalloys – Fundamentals and Applications (Cambridge University Press, Cambridge, 2006) [Google Scholar]
- J.J. Moverare, M. Segersäll, A. Sato, S. Johansson, R. Reed, Superalloys 2012, ed. E. S. Huron et al., 369 (2012) [CrossRef] [Google Scholar]
- G.M. Han, J.J. Yu, X.F. Sun, Z.Q. Hu, Mater. Sci. Eng. A, 528, 6217 (2011) [CrossRef] [Google Scholar]
- F. Liu, Z.G. Wang, S.H. Ai, Y.C. Wang, X.F. Sun, T. Jin, H.R. Guan, Scr. Mater., 48, 1265 (2003) [CrossRef] [Google Scholar]
- J.J. Moverare, S. Johansson, R.C. Reed, Acta Mater., 57, 2266 (2009) [Google Scholar]
- M. Segersäll, J.J. Moverare, K. Simonsson, S. Johansson, Superalloys 2012, ed. E. S. Huron et al., 215, (2012) [CrossRef] [Google Scholar]
- H.U. Hong, J.G. Yoon, B.G. Choi, I.S. Kim, Y.S. Yoo, C.Y. Jo, Int. J. Fatigue, DOI:10.1016/j.ijfatigue.2013.01.015 (2013) [Google Scholar]
- L. Kovarik, J. Unocic, J. Li, M.J. Mills, JOM, 61, 42 (2009) [CrossRef] [Google Scholar]
- L. Kovarik, J. Unocic, J. Li, P. Sarosi, C. Shen, Y. Wang, M.J. Mills, Prog. Mater. Sci., 54, 839 (2009) [CrossRef] [Google Scholar]
- M. Segersäll, J.J. Moverare, Materials, 6, 437 (2013) [CrossRef] [Google Scholar]
- M. Segersäll, J.J. Moverare, D. Leidermark, K. Simonsson, Metall. Mater. Trans. A, DOI:10.1007/s11661-014-2198-0 (2014) [Google Scholar]
- J.X. Zhang, H. Harada, Y. Ro, Y. Koizumi, T. Kobayashi, Acta Mater., 56, 2975 (2008) [CrossRef] [Google Scholar]
- A. Sato, J.J. Moverare, M. Hasselqvist, R.C. Reed, Metall. Mater. Trans. A, 43A, 2302 (2012) [CrossRef] [Google Scholar]