In- and out-of-phase thermomechanical fatigue of a Ni-based single-crystal superalloy
1 Department of Management and Engineering, Linköping University, 58183 Linköping, Sweden
2 Siemens Industrial Turbomachinery AB, 16283 Finspång, Sweden
a Corresponding author: This email address is being protected from spambots. You need JavaScript enabled to view it.
Abstract
In this study, the difference between in-phase (IP) and out-of-phase (OP) thermomechanical fatigue (TMF) cycling from 100 to 750 °C has been investigated for the Ni-based single-crystal superalloy MD2. In addition, two different crystal orientations were studied, the ⟨001⟩ and ⟨011⟩ orientations respectively. When comparing IP and OP TMF lives, a strain range dependency is found for the ⟨001⟩ direction. For high strain ranges, IP cycling leads to a higher number of cycles to failure compared to OP. However at lower strain ranges, OP cycling leads to a higher number of cycles to failure compared to IP. Microstructure investigation shows that for the ⟨001⟩ direction, deformation twinning within the γ/γ′-microstructure is much more pronounced during OP conditions compared to IP. However for the ⟨011⟩ direction, the opposite is observed; twinning is more pronounced during IP TMF. From the microstructure investigation it is also visible that intersections between twins seems to trigger formation of TCP phases and recrystallization. These intersections also work as initiation points for TMF damage.