Open Access
Issue
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
Article Number 21002
Number of page(s) 6
Section Posters: Mechanical Behavior III: Polycrystalline Alloys
DOI https://doi.org/10.1051/matecconf/20141421002
Published online 29 août 2014