Open Access
| Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 20002 | |
| Number of page(s) | 4 | |
| Section | Posters: Mechanical Behavior II: Single-Crystalline Alloys | |
| DOI | https://doi.org/10.1051/matecconf/20141420002 | |
| Published online | 29 août 2014 | |
- A. D. Cetel, D. N. Duhl, Superalloys 1988, 235 (1988) [CrossRef] [Google Scholar]
- K. Harris, G.L. Erickson, S.L. Sikkenga, W.D. Brentanall, J.M. Aurrecoechea, K.G. Kubarych, Superalloys 1992, 297 (1992) [Google Scholar]
- G.L. Erickson, Superalloys 1996, 35 (1996) [Google Scholar]
- W.S. Walston, L.S. O'Hara, E.W. Ross, T.M. Pollock, W.H. Murphy, Superalloys 1996, 27 (1996) [Google Scholar]
- J.X. Zhang, T. Murakumo, Y. Koizumi, T. Kobayashi, H. Harada, S. Masaki, Jr. Metall. Mater. Trans. A, 33A, 3741 (2002) [Google Scholar]
- Y. Koizumi, T. Kobayashi, T. Yokokawa, J. Zhang, M. Ogawa, H. Harada, Y. Aoki, M. Arai, Superalloys 2004, 35 (2004) [CrossRef] [Google Scholar]
- P.J. Fink, J.L. Miller, D.G. Konitzer, JOM, 62, 55 (2010) [CrossRef] [Google Scholar]
- J.B. Wahl, K. Harris, Superalloys 2012, 179 (2012) [Google Scholar]