- M.S.A. Karunaratne, P. Carter, R.C. Reed, Mat. Sci. Eng. A281, 229–233 (2000) [Google Scholar]
- R.A. Hobbs, M.S.A Karunaratne, S. Tin, R.C. Reed, C.M.F. Rae, Mat. Sci. Eng. A460-461, 587–594 (2007) [CrossRef] [Google Scholar]
- A. Heckl, S. Neumeier, M. Göken, R.F. Singer, Mat. Sci. Eng. A528, 3435–3444 (2011) [Google Scholar]
- A. Heckl, R. Rettig, R.F. Singer, Met. Mat. Trans A 41A, 202–211 (2010) [CrossRef] [Google Scholar]
- R.A. Hobbs, S. Tin, C.M.F. Rae, R.W. Broomfield, C.J. Humphreys, in Superalloys 2004 (The Minerals, Metals and Materials Society, Seven Springs, USA, 2004), pp. 819–825 [CrossRef] [Google Scholar]
- R. Darolia, D. Lahrman, R. Field, in Superalloys 1988 (The Metallurgical Society, Seven Springs, USA, 1988), pp. 255–264 [CrossRef] [Google Scholar]
- R.A. Hobbs, L. Zhang, C.M.F. Rae, S. Tin, Met. Mat. Trans. A 39A 1014–1025 (2008) [Google Scholar]
- C.M.F. Rae, R.C. Reed, Acta Mat. 49, 4113–4125 (2001) [Google Scholar]
- A.C. Yeh, S. Tin, Met. Mat. Trans. A 37, 2621–2631 (2006) [CrossRef] [Google Scholar]
- M.S.A. Karunaratne, C.M.F. Rae, R.C. Reed, Met. Mat. Trans. A 32A, 2409–2421 (2001) [Google Scholar]
- M. Simonetti, P. Caron, Mat. Sci. Eng. A254, 1–12 (1998) [CrossRef] [Google Scholar]
- K. Matuszewski, R. Rettig, M. Rasiński, K.J. Kurzydłowski, R.F. Singer, Adv. Eng. Mat. 16, 171–175 (2014) [CrossRef] [Google Scholar]
- A. Sato, H. Harada, T. Yokokawa, T. Murakumo, Y. Koizumi, T. Kobayashi, Scr. Mat 54, 1679–1684 (2006) [CrossRef] [Google Scholar]
- S. Neumeier, F. Pyczak, M. Göken, in Superalloys 2008, (The Minerals, Metals and Materials Society, Seven Springs, USA, 2008), pp. 109-119 [CrossRef] [Google Scholar]
- R. Rettig, A. Heckl, R.F. Singer, Adv. Mat. Res. 278, 180–185 (2011) [CrossRef] [Google Scholar]
- A.T.W. Kempen, F. Sommer, E.J. Mittemeijer, J. Mater. Sci 37, 1321–1332 (2002) [CrossRef] [Google Scholar]
- D.A. Porter, K.E. Easterling, M.Y. Sherif, Phase Transformations in Metals and Alloys, (CRC Press, Boca Raton, Fl, USA, 2009) [Google Scholar]
- R. Rettig, R.F. Singer, in Superalloys 2012, (The Minerals, Metals and Materials Society, Seven Springs, USA, 2012), pp. 205–214 [CrossRef] [Google Scholar]