Misorientation effect of grain boundary on the formation of discontinuous precipitation in second and third generation single crystal superalloys
1 National Centre for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083, China
2 Science and Technology on Advanced High Temperature Structural Material Laboratory, Beijing Institute of Aeronautical Materials, Beijing 100095, China
a Corresponding author: Cette adresse e-mail est protégée contre les robots spammeurs. Vous devez activer le JavaScript pour la visualiser.
Abstract
[001] tilt artificial grain boundaries of Ni-based single crystal superalloys CMSX-4 and DD10 have been prepared by self-diffusion bonding. The microstructural stability of 0 ∼ 30∘ artificial grain boundaries have been investigated after heat treatment at 1100 ∘C for 0 ∼ 300 h. TCP phases and cellular colony developed on boundaries are related to misorientation angle of the bonded boundaries of DD10 and DD10 alloys as well as the bonded boundaries of CMSX-4 and DD10 alloys. The heterogeneous nucleation of TCP phase, enveloped by γ′ film, occurred along 15∘ and 20∘ boundaries. Discontinuous Precipitation (DP) reaction occurred along high misorientation angle (20∘∼ 30∘) boundaries. However, no TCP phase formation existed along grain boundaries with different misorientation angles in CMSX-4/CMSX-4 bonded alloys as well as for a 0∘ boundary in DD10/DD10 and CMSX-4/DD10 bonded alloys. The current study clearly suggests that grain boundary precipitation and its morphology were influenced by the misorientation angle of grain boundary and the content of refractory elements in alloy.
© Owned by the authors, published by EDP Sciences, 2014
This is an Open Access article distributed under the terms of the Creative Commons Attribution License 4.0, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.