Open Access
Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
---|---|---|
Article Number | 11003 | |
Number of page(s) | 6 | |
Section | Posters: Precipitation | |
DOI | https://doi.org/10.1051/matecconf/20141411003 | |
Published online | 29 August 2014 |
- J.A. Dantzig, M. Rappaz. Solidification: CRC Press, Taylor & Francis Group, 2009 [CrossRef] [Google Scholar]
- N. Warnken, D. Ma, A. Drevermann, R.C. Reed, S.G. Fries, I. Steinbach, Acta Mater. 57, 5862, (2009) [CrossRef] [Google Scholar]
- C. Walter, B. Hallstedt, N. Warnken, Mat. Sci. Eng. A 397, 385, (2005) [CrossRef] [Google Scholar]
- C.A. Gandin, A. Jacot, Acta Mater. 55, 2539, (2007) [CrossRef] [Google Scholar]
- Q. Du, A. Jacot, Acta Mater. 53, 3479, (2005) [CrossRef] [Google Scholar]
- J.S. Langer, A.J. Schwartz, Phys. Rev. A, 21, 948, (1980) [CrossRef] [Google Scholar]
- I.M. Lifshitz, V.V. Slyozov. J. Phys. Chem. Solids 19, 35, (1961) [Google Scholar]
- C. Wagner. Z. Elektrochem. 65, 581, (1961) [Google Scholar]
- R. Kampmann, R. Wagner, In: Haasen P, Gerold V, Wagner R, Ashby Michael F, editors. Decomposition of Alloys: The Early Stages. Oxford: Pergamon Press, 1984, 91 [CrossRef] [Google Scholar]
- M. Perez, M. Dumont, D. Acevedo-Reyes. Acta Mater. 56, 2119, (2008) [CrossRef] [Google Scholar]
- P. Maugis, M. Gouné. Acta Mater. 53, 3359, (2005) [CrossRef] [Google Scholar]
- Q. Chen, J. Jeppsson, J. Agren. Acta Mater. 56, 1890, (2008) [CrossRef] [Google Scholar]
- H. Aaron, D. Fainstein, G. Kotler. J. Appl. Phys. 41, 4404, (1970) [CrossRef] [Google Scholar]
- L. Rougier, A. Jacot, C.-A. Gandin, P. Di Napoli, P.-Y. Théry, D. Ponsen, V. Jaquet, Acta Mater. 61, 6396, (2013) [CrossRef] [Google Scholar]
- C. Booth-Morrison, J. Weninger, C.K. Sudbrack, Z. Mao, R.D. Noebe, D.N. Seidman, Acta Mater. 56, 3422, (2008) [CrossRef] [Google Scholar]
- A. Jacot, M. Rappaz, Acta Mater. 50, 1909, (2002) [CrossRef] [Google Scholar]
- O.R. Myhr, Ø . Grong, Acta Mater. 48, 1605, (2000) [CrossRef] [Google Scholar]
- Ni20: Ni Base Alloys Database version NI20, http://www.thermocalc.com [Google Scholar]
- MobNi2: TCS Ni-alloys Mobility Database v2.0 http://www.thermocalc.com [Google Scholar]
- B.C. Wilson, E.R. Cutler, G.E. Fuchs, Mat. Sci. Eng. A 479, 356, (2008) [CrossRef] [Google Scholar]
- H. Ben Hamouda, PhD Thesis, MINES ParisTech-CEMEF, Sophia-Antipolis, France, 2012 [Google Scholar]
- C. Peyroutou, R. Tintiller, Internal report (1993) [Google Scholar]
- T. Grosdidier, A. Hazotte, A. Simon, Mat. Sci. Eng. A, 256, 183, (1998) [CrossRef] [Google Scholar]
- F. Diologent, P. Caron, Mat. Sci. Eng. A, 385, 245, (2004) [Google Scholar]