Modelling ternary effects on antiphase boundary energy of Ni3Al
Department of Materials Engineering Indian Institute of Science, Bangalore - 560012, India
a Corresponding author: This email address is being protected from spambots. You need JavaScript enabled to view it.
Abstract
The shearing of ordered γ′ precipitates by matrix dislocations results in the formation of antiphase boundaries (APB) in Ni-base superalloys. The APB energy is an important source of order-strengthening in disk and blade alloys where Ti and Ta substitute for Al in γ′. While the importance of APB energy is well-acknowledged, the effect of alloying on APB energy is not fully understood. In the present study, the effect of Ti and Ta additions on the {111} and {010} APB energies was probed via electronic structure calculations. Results suggest that at low levels of Ti/Ta, APB energies on either plane increases with alloying. However, at higher Ti/Ta levels, the APB energies decrease with alloying. These trends understood by accounting for nearest neighbour violations about the APB and additionally, invoking the effect of precipitate composition on the energy penalty of the violations. We propose an Environment Dependent Nearest Neighbour Bond (EDNNB) model that predicts APB energies that are in close agreement to calculated values.
© Owned by the authors, published by EDP Sciences, 2014