Probing the strain distribution within a single crystal superalloy during high temperature testing
1 Institut Jean Lamour (UMR CNRS-UL N ∘ 7198), Labex DAMAS, Parc de Saurupt, 54000 Nancy, France
2 LiPhy, 140 Avenue de la Physique, BP. 87, 38402 Saint-Martin-d'Hères, France
a Corresponding author: alain.jacques@univ-lorraine.fr
The combination of in situ high resolution diffraction experiments with synchrotron radiation and mechanical and diffraction modelling is used to investigate the microstructure and mechanical state of single crystal superalloys during high temperature tests: a very high temperature annealing without external load and a creep test.