Open Access
| Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 21004 | |
| Number of page(s) | 6 | |
| Section | Posters: Mechanical Behavior III: Polycrystalline Alloys | |
| DOI | https://doi.org/10.1051/matecconf/20141421004 | |
| Published online | 08 October 2014 | |
- M. Donachie, S. Donachie, Superalloys: A Technical Guide – 2nd edition, ASM International, 2002, pp. 37 [Google Scholar]
- D. Bettge, W. Österle, J. Ziebs, Z. Metallkd. 86 (1995) 3 [Google Scholar]
- J. Zýka, I. Andršová, B. Podhorná, B., K. Hrbáček, Proceedings of Metal 2013 [Google Scholar]