Open Access
| Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 09003 | |
| Number of page(s) | 6 | |
| Section | Session 9: Precipitation | |
| DOI | https://doi.org/10.1051/matecconf/20141409003 | |
| Published online | 29 August 2014 | |
- R. Kennedy, Superalloys 718 625 706 and Various Derivatives, 1–14 (2005) [CrossRef] [Google Scholar]
- R. Kennedy, W. D. Cao, T. Bayha, International Symposium on Niobium for High Temperature Applications (2003) [Google Scholar]
- M. Springmann, W. Rothkegel, D. Huenert, H. Schlums, 7th International Conference on Low Cycle Fatigue (2013) [Google Scholar]
- E. a. Ott, J. Groh, H. Sizek, Superalloys 718 625 706 and Various Derivatives, 35–45 (2005) [CrossRef] [Google Scholar]
- S. Oppenheimer, E. McDevitt, W. D. Cao, Superalloys 718 625 706 and Various Derivatives, 321–330 (2010) [Google Scholar]
- W. D. Cao, Superalloys 718 625 706 and Various Derivatives (2005) [Google Scholar]
- R. Cozar, A. Pineau, Metall. Mater. Trans. B, 4 (1973) [Google Scholar]
- L. Viskari, K. Stiller, Ultramicroscopy, 111, 652–8 (2011) [CrossRef] [Google Scholar]
- K. Löhnert, F. Pyczak, Superalloys 718 625 706 and Various Derivatives, 877–891 (2010) [Google Scholar]
- W. D. Cao, R. Kennedy, Superalloys, 3, 1–9 (2004) [Google Scholar]
- C. Stotter, Int. J. Mater. Res., 99, 376–380 (2008) [CrossRef] [Google Scholar]
- X. Xie, G. W. J. Dong, C. Xu, W. D. Cao, R. Kennedy, Superalloys 718 625 706 and Various Derivatives, 179–191 (2005) [Google Scholar]
- X. Xie, C. Xu, G. Wang, J. Dong, W. D. Cao, R. Kennedy, Mater. Res., 193–202 (2005) [Google Scholar]
- X. Xie, J. Dong, G. Wang, W. You, J. Du, C. Zhao, Z. Wang, T. Carneiro, Superalloys 718 625 706 and Various Derivatives, 3, 287–298 (2005) [CrossRef] [Google Scholar]
- E. Pickering, H. Mathur, A. Bhowmik et al., Acta Mater., 60, 2757-2769 (2012) [Google Scholar]
- O. Messé, J. Barnard, E. Pickering, P. Midgley, C. Rae, Philos. Mag., 94, 1132-52 (2014) [CrossRef] [Google Scholar]
- K. Löhnert, Dissertation, Universität Erlangen - Nürnberg, 2011 [Google Scholar]
- E. T. McDevitt, S. M. Oppenheimer, R. M. Kearsey, J. Tsang, Mater. Sci. Forum, 706–709, 2428–2433 (2012) [CrossRef] [Google Scholar]
- W. D. Cao, R. Kennedy, Allvac Technical Report, (2006) [Google Scholar]
- C. T. Sims, N. S. Stoloff, W. C. Hagel, Superalloys II. New York: John Wiley & Sons, 1987 [Google Scholar]
- W. Rasband, “ImageJ”, v1.44o, National Institutes of Health, USA [Google Scholar]
- Oxford Instruments, “HKL Channel 5”, v5.0.9.0 [Google Scholar]
- S. Ponnelle, B. Brethes, A. Pineau, Superalloys 718 625 706 and Various Derivatives, 92, 1–10 (2001) [Google Scholar]
- M. Detrois, R. Helmink, S. Tin, Mater. Sci. Eng. A, 586, 236–244 (2013) [CrossRef] [Google Scholar]
- G. J. Shiflet, M. A. Mangan, W. G. Meng, Interface Sci., 154, 133–154 (1998) [CrossRef] [Google Scholar]