Open Access
| Issue |
MATEC Web of Conferences
Volume 14, 2014
EUROSUPERALLOYS 2014 – 2nd European Symposium on Superalloys and their Applications
|
|
|---|---|---|
| Article Number | 07003 | |
| Number of page(s) | 6 | |
| Section | Session 7: Process - Microstructure Interactions | |
| DOI | https://doi.org/10.1051/matecconf/20141407003 | |
| Published online | 29 August 2014 | |
- C. Panwisawas, H. Mathur, J.-C. Gebelin, D.C. Putman, C.M.F. Rae, R.C. Reed, Acta Mater 61, 51 (2013)w [Google Scholar]
- G. Xie, L. Wang, J. Zhang, L.H. Lou, Metall Mater Trans A 39A, 206 (2008) [CrossRef] [Google Scholar]
- R. Burgel, P.D. Portella, J. Preuhs, Superalloys 2000 (TMS, Pennsylvania, 2000) [Google Scholar]
- U. Paul, P.R. Sahm, D. Goldschmidt, Mat Sci Eng A A173, 49 (1993) [CrossRef] [Google Scholar]
- R.C. Reed, The Superalloys: Fundamentals and Applications, p 139 (Cambridge University Press, Cambridge, 2006) [Google Scholar]
- D.C. Cox, B. Roebuck, C.M.F. Rae, R.C. Reed, Mater Sci Tech 19, 440 (2003) [CrossRef] [Google Scholar]
- G. Xie, L. Wang, J. Zhang, L.H. Lou, Scripta Mater 66, 378 (2012) [CrossRef] [Google Scholar]
- J.J. Moverare, S. Johansson, R.C. Reed, Acta Mater 57, 2266 (2009) [Google Scholar]
- L. Wang, F. Pyczak, J. Zhang, R.F. Singer, Int J Mater Res 100, 1046 (2009) [CrossRef] [Google Scholar]
- L. Wang, G. Xie, J. Zhang, L.H. Lou, Scripta Mater 55, 457 (2006) [CrossRef] [Google Scholar]
- A.J. Porter, B. Ralph, J Mater Sci 16, 707 (1981) [CrossRef] [Google Scholar]
- R.A. Hobbs, L. Zhang, C.M.F. Rae, S. Tin, Mat Sci Eng A 489, 65 (2008) [Google Scholar]
- W. Betteridge, Cobalt and its Alloys, p 74 (Horwood, Chichester, 1982) [Google Scholar]
- M.V. Nathal, L.J. Ebert, Metall Trans A 16A, 1849 (1985) [CrossRef] [Google Scholar]
- R.N. Jarrett, J.K. Tien, Metall Trans A, 13A, 1021 (1982) [CrossRef] [Google Scholar]
- R.A. Hobbs, R.A., S. Tin, C.M.F. Rae, Metall Mater Trans A 36A, 2761 (2005) [CrossRef] [Google Scholar]
- F.J. Humphreys, M. Hatherly, Recrystallization and Related Annealing Phenomena, p 16, 23 (Pergamon, Oxford, 1996) [Google Scholar]
- J.R. Davis, ed. Nickel, Cobalt, and their Alloys, p 349 (ASM International, Ohio, 2007) [Google Scholar]
- D.A. Hughes, W.D. Nix, Mat Sci Eng A 122, 153 (1989) [CrossRef] [Google Scholar]
- S.D. Bond, J.W. Martin, J Mater Sci 19, 3867 (1984) [CrossRef] [Google Scholar]
- R.M. Boothby, G.B. Merrill, 7th Riso International Symposium – Recovery, Recrystallization and Grain Growth (Riso National Laboratory, Roskilde, 1986) [Google Scholar]