Development and use of a new burner rig facility to mimic service loading conditions of Ni-based single crystal superalloys
1 Institut Pprime, CNRS, ENSMA, Université de Poitiers, UPR CNRS 3346, Physics and Mechanics of Materials Department, ENSMA, Téléport 2, 1 avenue Clément Ader, BP. 40109, 86961 Futuroscope Chasseneuil Cedex, France
2 Safran – Turbomeca, Avenue Joseph Szydlowski, 64511 Bordes Cedex, France
a Corresponding author: This email address is being protected from spambots. You need JavaScript enabled to view it.
Abstract
Performing representative experiments of in-service operating conditions of Ni-based superalloys used as high pressure turbine blades in aeroengines is a challenging issue due to the complex environmental, mechanical and thermal solicitations encountered by those components. A new burner rig test facility called MAATRE (French acronym for Mechanics and Aerothermics of Cooled Turbine Blades) has been developed at ENSMA – Pprime Institute to mimic as close as possible those operating conditions. This new test bench has been used to perform complex non-isothermal creep tests representative of thermomechanical solicitations seen by some sections of HP turbine blades during engine certification procedure.
© Owned by the authors, published by EDP Sciences, 2014