Effect of solidification parameters on the secondary dendrite arm spacing in MAR M-247 superalloy determined by a novel approach
1 IMDEA Materials Institute, C/ Eric Kandel 2, 28906 Getafe, Madrid, Spain
2 Precicast Bilbao, S.A. El Barracón 1, 48901 Barakaldo (Bizkaia), Spain
a Corresponding author: This email address is being protected from spambots. You need JavaScript enabled to view it.
Abstract
The effect of solidification parameters on the secondary dendrite arm spacing in a MAR-M247 Ni-based superalloy has been studied by a novel approach, based on physical simulation of melting/solidification experiment with a constant cooling rate and variable temperature gradient. The applied experimental method proved to be efficient as it yielded a spread of microstructures corresponding to a range of well controlled solidification rates in a single melting/solidification experiment. In addition, it has been demonstrated that secondary dendrite arm spacing is better related to the solidification rate than to the cooling rate in the case when significant variations of thermal parameters during the solidification process occur.
© Owned by the authors, published by EDP Sciences, 2014