Turbine blades production technique equipment built with a glance of high-gradient directional crystallization process nature
FSUE “All Russian Scientific Research Institute of Aviation Materials” (VIAM), 105005, Radio str. 17, Moscow, Russia
Abstract
The influence of the high-gradient directional crystallization on the structural components (the interdendritic distance and porosity) of the superalloys is presented in the Article. The industrial-scale high-gradient plant of UVNS-6 type and some benefits of its use are shown here as well. Some test specimens manufactured on the UVNS-6 are studied with measurement of the interdendritic distance. The temperature gradient is estimated by experimental method.
© Owned by the authors, published by EDP Sciences, 2014